Knead and shape your own designs with classic ceramic clay.
A finished product needs to dry up to 24 hours in an open air, normal temperature environment without shrinking or bending
To get porcelain, leave to dry completely before product is fired in kiln 1000-1300 degrees celcius
Can be used for decorative purposes if air dried only.
Finished product can be painted and varnished.